Tuesday, March 9, 2010

The Making of a New Mold

The following sequence of photos shows a few of the many steps required to make a mold from RTV Silicone.

The first 3 photos shows the hard master. This master was machined from hard plastic and has been fastened to the base. Both the master and the base have been coated to make them as slick and shiny as possible. The smoother and shinier the master the shinier the castings the mold will produce. Hours of time and effort go into this part of the process and after the mold is made, these parts will not used again.

The 4th photo shows the master after the mold box has been built around it. I made this box as small as possible because this mold will only be used for very few castings, so thick walls around the master were not necessary. As long as I support the walls to prevent deflection during the casting process, this mold will give satisfactory results. The reason for the thin walls is to use as little RTV silicone as possible. The intent of this mold is to replicate the hard master with several copies that are identical. These multiple copies will then be used to make a multi cavity production mold.

With the master and the mold box ready, its time to mix the silicone. This particular RTV is a 10 to 1 mix. 10 parts of RTV to 1 part catalyst, by weight. In order to get the proper mix I weigh the RTV and then add the correct amount of catalyst.
Photo 5 shows the RTV.
Photo 6 is after the catalyst is added.
Photo 7 is the beginning to the mixing process. You must mix the two parts until a consistent color is reached.
Photo 8 shows the mixed RTV and ready to be poured into the mold box. You can see the RTV de-gassing itself by the presence of air bubbles coming to the top. This de-gassing will continue for quite some time and will cause no problems in the mold as long as none of the bubbles gets trapped against the master as the RTV cures.

Photo 9 through 12 shows the RTV being slowly poured into the mold box until the master is completely submerged.

Now we wait. It takes about 24 hours for the RTV to cure before we can remove the master to see how our new mold turned out.
I'll post some more of this process in a later post.
















Sunday, March 7, 2010

A little time on the water, Finally

My cousin and I got out for a little while today. It sure felt good to finally be able to get out on the water. We did manage catch a few Sauger which was a very nice bonus considering the water temps are still in the 30's. Being able to get out and catch a few fish gives me hope that spring may actually be just around the corner.
Posting some fish photos, even though small, is a welcome change from all the bait pics I've been posting.






Friday, March 5, 2010

Big Game Twitch Baits and a Hughes River

A friend sent me these two 7" and two 9" unpainted Big Game blanks along with a 7" Big Game and a 8" Hughes River that had been used, abused and chewed.
The first three photos are how they looked when I received them, The next two photos are the used baits after I stripped off the original finish. The last five are how they looked after they came off the drying wheel.
They are soon to be on their way back to him, hopefully he will send me some photos of some impressive muskies he gets on them.








Wednesday, March 3, 2010

Big Boys

A few more colors
Real Perch
Mean Streak
Red Sucker
Blue Shad
Tennessee Shad Orange Belly
Pink Shad
Alandsfargen
Atomkrullen
Dirty Roach
Orange Perch








Monday, March 1, 2010

A Few Colors of Big Boy Swimbaits

Hot Bluegill
Hot Crazy Northern Lights
Bluegill
Yellow Pikie
Coward
Chartreuse Shiner
Dr. Carp
Chartreuse Red Head
Fish Food
Old Pike